This site is not affiliated with AGCO Inc., Duluth GA., Allis-Chalmers Co., Milwaukee, WI., or any surviving or related corporate entity. All trademarks remain the property of their respective owners. All information presented herein should be considered the result of an un-moderated public forum with no responsibility for its accuracy or usability assumed by the users and sponsors of this site or any corporate entity. | |||||
The Forum | Parts and Services | Unofficial Allis Store | Tractor Shows | Serial Numbers | History |
Couple electrolysis questions. |
Post Reply ![]() |
Page <12 |
Author | |
CTuckerNWIL ![]() Orange Level ![]() ![]() Joined: 11 Sep 2009 Location: NW Illinois Points: 22823 |
![]() ![]() ![]() ![]() ![]() |
Tom, It is best if you can get a large surface area of the part facing the largest surface of the anode. Hanging the part also makes it easier to rotate to get the "dirty" side to face the anode.
|
|
http://www.ae-ta.com
Lena 1935 WC12xxx, Willie 1951 CA6xx Dad bought new, 1954WD45 PS, 1960 D17 NF |
|
![]() |
|
Sponsored Links | |
![]() |
|
TomYaz ![]() Orange Level ![]() ![]() Joined: 14 Sep 2009 Location: PA Points: 10325 |
![]() ![]() ![]() ![]() ![]() |
Thanks Chuck and Lou.
Having the part hang will be impractical for some of these parts so I am willing to have slower clean rate, just want to be sure it will still work. Dont mind flipping and repositioning the part...
|
|
![]() |
|
jjrosty ![]() Silver Level ![]() Joined: 15 Sep 2009 Location: Broken Arrow OK Points: 106 |
![]() ![]() ![]() ![]() ![]() |
THe same guy that is cleaning the old wood machines also told me "Black to the Bailey" as in planes. so the black always goes to what your cleaning.
I didn't think AC current would work? |
|
![]() |
|
Matt MN ![]() Orange Level ![]() ![]() Joined: 14 Sep 2009 Location: Silver lake MN Points: 1491 |
![]() ![]() ![]() ![]() ![]() |
I have not tried this yet but would like to. Is the part to be cleaned the positive or negative from the charger?
|
|
Unless your are the lead horse the scenery never changes!!
|
|
![]() |
|
Rawleigh ![]() Orange Level ![]() ![]() Joined: 14 Sep 2009 Location: White Stone, VA Points: 421 |
![]() ![]() ![]() ![]() ![]() |
Neg to the part!! I use a 250 gallon tote with the top cut out of it.
|
|
![]() |
|
Boomer ![]() Bronze Level ![]() Joined: 13 Sep 2009 Location: Mid Missouri Points: 102 |
![]() ![]() ![]() ![]() ![]() |
Has anybody tried it on a much larger scale. Like a whole body of a military jeep? What happens if there is bondo on the metal? How quick do you paint after use this method?
|
|
![]() |
|
Boomer ![]() Bronze Level ![]() Joined: 13 Sep 2009 Location: Mid Missouri Points: 102 |
![]() ![]() ![]() ![]() ![]() |
What happens if you have bronze bushings?
|
|
![]() |
|
Lance/SC ![]() Orange Level ![]() Joined: 14 Sep 2009 Location: Lexington, SC Points: 411 |
![]() ![]() ![]() ![]() ![]() |
Rawleigh, what do you use for anodes and what how far apart are they? Got any Pics?
|
|
![]() |
|
Rawleigh ![]() Orange Level ![]() ![]() Joined: 14 Sep 2009 Location: White Stone, VA Points: 421 |
![]() ![]() ![]() ![]() ![]() |
I am using some old metal shelving. I used four at a time, one on each side. I made jumpers from wire and battery clips to string them together. I put a cinder block in the bottom to keep the part up off the floor.
I have heard of a person digging a pit and lining it with plastic to do trailer frames. They used a DC welder for that job. |
|
![]() |
|
TomYaz ![]() Orange Level ![]() ![]() Joined: 14 Sep 2009 Location: PA Points: 10325 |
![]() ![]() ![]() ![]() ![]() |
Ok I started mine around 5:30 PM last night.
Used a 50 gal ruubermaid plastic tank waterer.
Used lye instead of washing soda...
For sacrificial anodes I bracketed the allcrop 60 piece with two MF plow landsides ..(with pleasure heheh)
Rested part on bottom of tank, no "hanging" I believe the plastic serves as an insulator from the other side of the equation.
Seems to work great...can hear the fizzing crazy like an just opened can of soda!
12 hours later is still fizzing; working on the rust...
Here is a formula I found that supposedly works even better:
Sodium Carbonate (washing soda) 75 grams/liter 10 0unces/U.S. gal.
Sodium Hydroxide (lye)__________12.5__________1.7 Trisodium Phosphate (TSP)_______25___________3.3 Sodium Silicate (water-glass)_____12.5__________1.7 Lucky for me I have a gallon of water glass laying around...(doesnt everyone?)
Will have to try this formula some time
Edited by TomYaz - 20 Sep 2010 at 11:59am |
|
![]() |
|
clovis ![]() Orange Level ![]() Joined: 11 Sep 2009 Points: 384 |
![]() ![]() ![]() ![]() ![]() |
This has been a great thread...I've always wanted to try this method...thanks for the great posts everyone.
|
|
![]() |
Post Reply ![]() |
Page <12 |
Tweet
|
Forum Jump | Forum Permissions ![]() You cannot post new topics in this forum You cannot reply to topics in this forum You cannot delete your posts in this forum You cannot edit your posts in this forum You cannot create polls in this forum You cannot vote in polls in this forum |